Invar 36 (Invar36)

›

Basic Properties

Alloy Type
Designation Invar36
Density 8.05 g/cm³
Melting Point 1427°C

Composition

Element Percentage

Description

Iron-nickel alloy with extremely low coefficient of thermal expansion near room temperature.
Density 8.05 g/cm³
Electrical Resistivity 82 μΩ·cm
Tensile Strength 440-540 MPa
Yield Strength 260-340 MPa
Elongation 30-45%
Hardness 140-200 HB
Machinability Good - machines well with standard tooling
Melting Point 1427°C
Thermal Conductivity 10.7 W/(m·K)
Thermal Expansion 1.5 μm/(m·K)
Heat Treatment Stress relief at 315°C, not heat treatable for strengthening
Heat Treatment Stress relief at 315°C, not heat treatable for strengthening
Corrosion Resistance Fair - iron-nickel alloys require protection from corrosion

Applications

Precision instruments, measuring tapes, pendulum rods, bimetallic strips, clock components

History

Discovered by Charles Guillaume in 1896, earned him Nobel Prize in Physics.