Stainless Steel 15-5 PH (15-5PH)

›

Basic Properties

Alloy Type
Designation 15-5PH
Density 7.8 g/cm³
Melting Point 1400-1440°C

Composition

Element Percentage

Description

Precipitation-hardening martensitic stainless steel with high strength and good corrosion resistance.
Density 7.8 g/cm³
Electrical Resistivity 80 μΩ·cm
Tensile Strength 1000-1380 MPa
Yield Strength 930-1280 MPa
Elongation 6-16%
Hardness 28-47 HRC
Machinability Good in annealed condition, more difficult when aged
Melting Point 1400-1440°C
Thermal Conductivity 16.8 W/(m·K)
Thermal Expansion 10.8 μm/(m·K)
Heat Treatment Solution treatment at 1040°C + aging at 480°C for 4 hours
Heat Treatment Solution treatment at 1040°C + aging at 480°C for 4 hours
Corrosion Resistance Good - similar to 17-4 PH with slightly better corrosion resistance

Applications

Aerospace components, nuclear applications, chemical processing, valve components

History

Development of 17-4 PH with improved corrosion resistance.