A-286 (A286)

›

Description

An austenitic precipitation-hardening stainless steel with good creep resistance up to 700°C
No physical properties data available
No mechanical properties data available
No thermal properties data available
No processing properties data available

Applications

Jet engine components, high-temperature bolts, gas turbine parts, nuclear applications