Mu-metal (Mu-80)
›
Basic Properties
| Alloy Type | |
|---|---|
| Designation | Mu-80 |
Description
A nickel-iron alloy with extremely high magnetic permeability, ideal for shielding
| No physical properties data available |
| No mechanical properties data available |
| No thermal properties data available |
| No processing properties data available |
Applications
Magnetic shielding, sensitive electronic equipment protection, MRI rooms