Basic Properties

Alloy Type
Designation D2
Density 7.7 g/cm³
Melting Point 1420-1460°C

Composition

Element Percentage

Description

A high-carbon, high-chromium air-hardening tool steel with excellent wear resistance and dimensional stability
Density 7.7 g/cm³
Electrical Resistivity 95 μΩ·cm
Tensile Strength 1520-2070 MPa
Yield Strength 1380-1720 MPa
Elongation 2-8%
Hardness 450-650 HV
Machinability Good machinability in annealed condition. Requires carbide tools when hardened.
Melting Point 1420-1460°C
Thermal Conductivity 19 W/(m·K)
Thermal Expansion 11.2 × 10⁻⁶/°C
Heat Treatment Annealing at 870-900°C, hardening at 1010-1030°C, tempering at 150-540°C
Heat Treatment Annealing at 870-900°C, hardening at 1010-1030°C, tempering at 150-540°C
Corrosion Resistance Moderate corrosion resistance due to chromium content. Better than carbon tool steels.

Applications

Stamping dies, blanking dies, forming tools, shear blades, punches, industrial knives

History

Developed for improved wear resistance and air hardening capability.